Thread: how to measure depth of pitting corrosion?

  1. #1
    mina1227
    Guest

    how to measure depth of pitting corrosion?

    we have stainless steel tank that wear out over time from viberation, and starts to get pitting corrosion. any one know of a good way to measure the depth of the corroted areas?

  2. #2
    Technical Fellow Kelly_Bramble's Avatar
    Join Date
    Feb 2011
    Location
    Bold Springs, GA
    Posts
    2,619
    There are a variety of methods for measuring pit depth. Ultrasonically, mechanically, etc.

    Depth gauge with small stylus:

    pit-measurement.jpg

  3. #3
    Senior Engineer
    Join Date
    Sep 2014
    Posts
    34
    wow nice information regarding the corrosion.We can measure the deapth of pitting corrosion. This is a very nice stuff. Thanks.