Mechanical Design, Manufacturing and Engineering Forum
[ Home ] [ Search ] [ Engineering and Design Database ] [ Resume/Job Database ] [ Product and Services Directory ]
[
Engineering, Design and Drafting Store ] [ Engineering Forum ] [ DFM DFA Training and Trainers ] [ GD&T Training GD&T Trainers ] [ Advertise ]
[ POSTING POLICY / RULES ][ Archive#1 ] [ Archive #2 ] [ Archive #3] [ Calculators ] [ Tell A Friend ]
Forum Moderators: randykimball, Administrator

plating surface preparation
Post Reply   Forum
Posted by: gwood

03/29/2005, 16:51:54

Author Profile Mail author Edit
Hi. Any thoughts would be greatly appreciated on the following:
1) Would placing machined Ti-6Al-4V in a bath of HBF(4)/HCl and then aqueous ultrasonic cleaning present risk for subsequent hydrogen embrittlement or other problems?


2) Any thoughts on cleaning a machined Ti-6Al-4V surface to prepare for nickel plating?

Thanks, have a good day.